Mechanical Properties Metric English Comments
Compressive Modulus 19.3 GPa

@Temperature 23.9 °C
2800 ksi

@Temperature 75.0 °F
Dry; 8HS form; ASTM D695
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Compressive Modulus 19.3 GPa

@Temperature 23.9 °C
2800 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced
Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s..