Polymer Property : Compressive Modulus = 18.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 18.6 GPa

@Temperature 23.9 °C
2700 ksi

@Temperature 75.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Compressive Modulus 18.6 GPa
2700 ksi
ASTM D695
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap..