Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.20 GPa | 174 ksi | Unloading, In the In Plane Direction |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Compressive Modulus | 1.20 GPa | 174 ksi | Unloading, In the Foaming Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |