Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.03 GPa | 150 ksi | TM R050-38 |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Compressive Modulus | 1.03 GPa | 150 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 1.03 GPa | 150 ksi | Stabilized, typ |
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Modulus | 1.03 GPa | 150 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.03 - 35.0 GPa | 150 - 5080 ksi | Average value: 8.95 GPa Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Compressive Modulus | 1.03 GPa | 150 ksi | TM R050-38 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Compressive Modulus | 1.03 GPa | 150 ksi | TM R050-38 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |