Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.104 GPa | 15.1 ksi | |
Sawbones Second-Generation Simulated Cancellous Bone (Solid) Rigid Polyurethane BoneSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ma.. |
|||
Compressive Modulus | 0.104 GPa | 15.1 ksi | |
Sawbones Third-Generation Simulated Cancellous Bone (Solid) Rigid Polyurethane BoneSawbones® standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid.. |
|||
Compressive Modulus | 0.104 GPa | 15.1 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Compressive Modulus | 0.104 - 0.155 GPa | 15.1 - 22.5 ksi | Average value: 0.133 GPa Grade Count:3 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |