Polymer Property : Compressive Modulus = 14.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 12.1 - 14.7 GPa
1750 - 2130 ksi
Average value: 13.4 GPa Grade Count:3
Overview of materials for Phenolic, Graphite Cloth Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value..