Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | >= 0.100 GPa | >= 14.5 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |