Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.931 GPa | 135 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 0.931 GPa | 135 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 0.931 GPa | 135 ksi | ASTM D-695 |
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h.. |