Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 8.41 - 17.0 GPa | 1220 - 2470 ksi | Average value: 11.9 GPa Grade Count:3 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Compressive Modulus | 8.41 GPa | 1220 ksi | |
Phenolic 46%, Carbon fabric 54% Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA" |