Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.731 GPa | 106 ksi | Stabilized, typ, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 3/8 - 7.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |