Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0689 GPa | 10.0 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 0.0690 - 0.114 GPa | 10.0 - 16.5 ksi | |
ERG Aerospace Duocel® Aluminum Metal Foam |
|||
Compressive Modulus | 0.0690 GPa | 10.0 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |