Mechanical Properties Metric English Comments
Compressive Modulus 0.00940 GPa
1.36 ksi
0.1; ASTM D695
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.