Polymer Property : Compressive Modulus = 0.856 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.000200 - 0.00590 GPa
0.0290 - 0.856 ksi
Average value: 0.00208 GPa Grade Count:10
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..