Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00420 GPa | 0.609 ksi | 0.1; ASTM D695 |
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |