Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00400 GPa | 0.580 ksi | at 15% Compression; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2550 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Compressive Modulus | 0.00400 GPa | 0.580 ksi | at 15% Compression; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |