Polymer Property : Compressive Modulus = 0.531 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.531 GPa
77.0 ksi
ASTM D695
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet)
Compressive Modulus 0.531 GPa
77.0 ksi
ASTM D695
Saint-Gobain Fluoroloy® A09 High Performance Seal Material
Extremely tough, long-wearing material; Excellent in water and water-based fluids, particularly suitable for abrasive media; Long wear life under severe conditions; Limited heat and chemical resista..