Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00196 GPa | 0.284 ksi | 10% Compression Modulus; ASTM D695 |
Toyobo Pelprene™ P-30B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Compressive Modulus | 0.00196 - 0.0350 GPa | 0.284 - 5.08 ksi | Average value: 0.0138 GPa Grade Count:4 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |