Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.1375 GPa | 19.94 ksi | |
Sawbones Cellular Rigid Polyurethane Foam 20 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |