Mechanical Properties Metric English Comments
Compressive Modulus 0.137 GPa
19.9 ksi
Cellular; ASTM D1621
Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone)
Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rig..
Compressive Modulus 0.137 GPa
19.9 ksi
Sawbones Second-Generation Simulated Cancellous Bone (Cellular)
Rigid Polyurethane BoneSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ma..
Compressive Modulus 0.137 GPa
19.9 ksi
Sawbones Third-Generation Simulated Cancellous Bone (Cellular)
Rigid Polyurethane BoneSawbones® standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid..