Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0850 GPa | 12.3 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Compressive Modulus | >= 0.0850 GPa | >= 12.3 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |