Polymer Property : Compressive Modulus = 0.0720 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0720 GPa

@Thickness 19.0 mm
10.4 ksi

@Thickness 0.750 in
perpendicular to plane; ASTM C365
3A Composites Core Materials AIREX® PXw.320 Fiber-Reinforced Structural Foam Panel
AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou..