Mechanical Properties Metric English Comments
Compressive Modulus 0.0620 GPa
8.99 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..