Compressive Modulus 0.0500 GPa
7.25 ksi
At 15% Compression; ISO 7743
Premix Thermoplastics PRESEAL® TPE 6071
PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp..
Compressive Modulus 0.0500 GPa
7.25 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Compressive Modulus >= 0.0500 GPa
>= 7.25 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..