Polymer Property : Compressive Modulus = 0.0350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0350 GPa
5.08 ksi
10% Compression Modulus; ASTM D695
Toyobo Pelprene™ P-280B Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
Compressive Modulus >= 0.0350 GPa
>= 5.08 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Compressive Modulus >= 0.0350 GPa
>= 5.08 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..