Polymer Property : Compressive Modulus = 0.0330 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0330 GPa
4.79 ksi
At 10% Compression; ISO 7743
Premix Thermoplastics PRESEAL® TPE 5010
PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica..