Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0107 GPa | 1.55 ksi | |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |