Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.000124 GPa | 0.0180 ksi | Force to Compress, Value given for 25% compression; ASTM D1667 |
Saint-Gobain Korel® K40-20 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |