Polymer Property : Graves Tear Strength = 23.6 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 23.6 kN/m

@Temperature 23.0 °C
135 pli

@Temperature 73.4 °F
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..