Mechanical Properties Metric English Comments
Graves Tear Strength 10.2 kN/m

@Temperature 100 °C
58.2 pli

@Temperature 212 °F
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber  (discontinued **)
A black thermoplastic general purpose elastomer designed for thin wall extrusion with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo..