Mechanical Properties Metric English Comments
Compressive Yield Strength 970 MPa
141000 psi
0.2%, hardened to 30 HRC
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha..