Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 89.6 - 97.0 MPa | 13000 - 14100 psi | Average value: 94.9 MPa Grade Count:8 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Compressive Yield Strength | 34.0 - 97.0 MPa | 4930 - 14100 psi | Average value: 79.5 MPa Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |