Mechanical Properties Metric English Comments
Compressive Yield Strength 6.65 MPa
965 psi
Bare, typ, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..