Mechanical Properties Metric English Comments
Compressive Yield Strength 9.2210 MPa
1337.4 psi
Stress at 3% Strain; ASTM D6108-97
Plastic Lumber from the Plastic Lumber Co.
Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep..