Polymer Property : Compressive Yield Strength = 870 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 6.00 MPa
870 psi
at 1% nominal strain; ISO 604
Quadrant EPP Cestilene™ HD 1000 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 6.00 MPa

@Strain 1.00 %
870 psi

@Strain 1.00 %
ISO 604
Manifattura Cattaneo PE UMW Polyethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Compressive Yield Strength 6.00 - 96.5 MPa
870 - 14000 psi
Average value: 48.0 MPa Grade Count:7
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Compressive Yield Strength 6.00 - 162 MPa
870 - 23500 psi
Average value: 66.0 MPa Grade Count:42
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Compressive Yield Strength 6.00 - 7.00 MPa

@Strain 1.00 %
870 - 1020 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..