Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 87.6 MPa | 12700 psi | ASTM D695 |
Devcon Fastmealâ„¢ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |