Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.14 MPa | 745 psi | Stabilized, typ |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Designation: Material-Cell Size-Density.Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the.. |