Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 7.20 MPa | 1040 psi | ASTM D695 |
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |