Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 68.95 MPa | 10000 psi | |
Abatron AboCast 8103-16 One Part Epoxy One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak e.. |