Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 450 MPa | 65300 psi | at 5% deformation, parallel to thickness |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |