Mechanical Properties Metric English Comments
Compressive Yield Strength 0.450 MPa
65.3 psi
at 10% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.450 MPa
65.3 psi
Static, 70% Compression, ASTM D1621
Covestro Bayfill® EA 4004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Compressive Yield Strength 0.450 MPa
65.3 psi
Compressive Load Deflection at 20%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..