Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 603 MPa | 87500 psi | |
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |