Polymer Property : Compressive Yield Strength = 57.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 57.0 MPa
8260 psi
ASTM D695
Devcon Plastic Steel® Putty (A) Epoxy
General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. ..