Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 365 MPa @Temperature 23.0 °C |
52900 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 365 MPa | 52900 psi | |
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |