Mechanical Properties Metric English Comments
Compressive Yield Strength 29.0 - 34.5 MPa
4200 - 5000 psi
Average value: 32.1 MPa Grade Count:4
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..