Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0350 - 0.0830 MPa
5.08 - 12.0 psi
at 25% deflection; 0.2"/min strain rate
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Compressive Yield Strength 0.0350 - 0.0650 MPa
5.08 - 9.43 psi
25% Compression
BIW ASTM Class 2D2 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...