Compressive Yield Strength | >= 331 MPa | >= 48000 psi | Compressive yield will be 1.2 times the tensile yield |
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |