Polymer Property : Compressive Yield Strength = 460 MPa
Polymer Property :
Compressive Yield Strength =
460 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Yield Strength
460
MPa
66700
psi
90º, RT, Dry; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel