Polymer Property : Compressive Yield Strength = 42.1 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.290 MPa
42.1 psi
Parallel to thickness @ 10% compression
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Compressive Yield Strength 0.290 MPa
42.1 psi
at 5% compression, parallel to thickness
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION
ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a..
Compressive Yield Strength 0.290 MPa
42.1 psi
Parallel to thickness @ 10% compression
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..