Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 41900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 289 MPa
41900 psi
ASTM D695
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap..
Copyright © lookpolymers.com All Rights Reserved