Polymer Property : Compressive Yield Strength = 4.35 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0300 MPa
4.35 psi
at 10% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ M DM-710A Foam Polyurethane
MDI backbone: ether.Shore 00 Hardness: 55Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Compressive Yield Strength 0.0300 MPa
4.35 psi
at 10% Compression, Parallel to thickness
Zircar Ceramics AXHTM Alumina-Silica Insulation
ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a..
Compressive Yield Strength 0.0300 MPa

@Strain 25.0 %
4.35 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Evacell EVA 50/S EVA + NR Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..